Submerge Arc MIG Welding Wire Em12

Product Details
Customization: Available
Type: Rolling Wire
Material: Low Carbon Steel
Still deciding? Get samples of US$ 0/Piece
Request Sample
Manufacturer/Factory, Trading Company

360° Virtual Tour

Diamond Member Since 2018

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Importers and Exporters
The supplier has import and export rights
High Repeat Buyers Choice
More than 50% of buyers repeatedly choose the supplier
Self-branded
The supplier has 2 Self-brands, check the Audit Report for more information
Patents Awarded
The supplier had awarded 1 patents, you can check the Audit Report for more information
to see all verified strength labels (25)
  • Submerge Arc MIG Welding Wire Em12
  • Submerge Arc MIG Welding Wire Em12
  • Submerge Arc MIG Welding Wire Em12
  • Submerge Arc MIG Welding Wire Em12
  • Submerge Arc MIG Welding Wire Em12
  • Submerge Arc MIG Welding Wire Em12
Find Similar Products

Basic Info.

Model NO.
EM12
Flux Containing
Not Containing Flux
Slag Characteristic
Acidic
Extended Length
10-20mm
Transport Package
Pallet
Specification
25kg, 50kg, 200kg, 250kg
Trademark
OEM
Origin
China
HS Code
8311100000
Production Capacity
1800 Tons Per Month

Product Description

Submerge Arc MIG Welding Wire Em12
1. Description: 
1)The weld metal shows a Fine appearance.
2) Both AC and DC can be applied.
3)Stable Arc
4)Easily removable residue

The products easily removable residue, good seam forming and highly efficient deposiyion. Wire meltingdoes not lead to splash or strong flasing. The sem surface is smooth and welding quality is guaranteed. They facilitate mechanical and automatic welding process. With a wide range of welding parameters, the wires can be used in open fields with strong wind and applied to automobiles, ships, bridges and chemical engineering.

Main Applications:
It is suitable to weld 450Mpa-500Mpa grade structures, such as boilers, ships, bridges, pressure vessels, as well as LPG cylinders, Before welding, the base metal must clear away impurities and fht flux must be baked in a temperature of 300° C-350° C for 1-2 hours.
                                                                       Mechanical  Property
    Joint  Strength
                (MPA)δ
succumb  strength
    (MPA)  δ 0.2
elongation  index
                  δ 5%
shock  value
            Akv
            -20  (J)

 

 

 
                    560                 480                     30         105
 

 

 

 

 

 

 

 

 

 
                                                                         Chemical  Composition
                                C                       Mn                           Si               S     P
 
Other
                        0.07%                   0.95%                     0.03%         0.010% 0.012%
 
≤ 0.50

 

 

 

 

 

 

 
                                                                                        Procedure& Package
Dia            2.0mm            2.5mm       3.0mm    3.2mm     4.0mm    5.0mm
Current            300-400           350-450    400-500 425-525 475-575 550-650
Voltage              26-29            27-30       27-30   27-30     27-30 27-30
Weight/spool(KG)                25              25          25    25     25 25
 
Submerge Arc MIG Welding Wire Em12
Submerge Arc MIG Welding Wire Em12
Our Factory and Production Line: 
Submerge Arc MIG Welding Wire Em12
The package of  Submerged Arc Welding Wire:more than 250kg / pallet
Submerge Arc MIG Welding Wire Em12

We assist in Beijing Essen Welding&Cutting Fair each year.
Submerge Arc MIG Welding Wire Em12

FAQ
Q1: Can I have a sample for testing? 
A: Yes, we can support free sample
Q2: Can I add my logo on the boxes/cartons? 
A: Yes, OEM and ODM are available from us. 
Q 3: What are the benefits of being a distributor? 
A: Special discount Marketing protection
Q4: Do you have inspection procedures for welding wires? 
A: 100% self-inspection before packing. We provide Quality Certification for every order. 
Q5: Can we mix itmes in one 20FT container? 
A: Yes
Q6: Can I have a visit to your factory before the order? 
A: Sure, welcome your visit of factory. 
 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier