• Widely Used Aluminum Alloy Wire Er4043, Er5356, Er5183, Er4047
  • Widely Used Aluminum Alloy Wire Er4043, Er5356, Er5183, Er4047
  • Widely Used Aluminum Alloy Wire Er4043, Er5356, Er5183, Er4047
  • Widely Used Aluminum Alloy Wire Er4043, Er5356, Er5183, Er4047
  • Widely Used Aluminum Alloy Wire Er4043, Er5356, Er5183, Er4047
  • Widely Used Aluminum Alloy Wire Er4043, Er5356, Er5183, Er4047

Widely Used Aluminum Alloy Wire Er4043, Er5356, Er5183, Er4047

Type: Rolling Wire
Material: Aluminum / Aluminum Alloy
Flux Containing: Not Containing Flux
Slag Characteristic: Acidic
Extended Length: 10-20mm
Transport Package: Carton
Samples:
US$ 0/kg 1 kg(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2018

Suppliers with verified business licenses

Manufacturer/Factory, Trading Company

Basic Info.

Model NO.
ER4043, ER5356, ER5183, ER4047
Specification
6~7kg/caron, 5kg/tube
Trademark
OEM
Origin
China, Shangdong

Product Description

This type of product is widely used as general welding material with the magnesium of 5% and a little of Titanium fine grains. And this product is of high toughness, good forgeability, and well anti-corrosiveness, Furthermore, it's a good choice for color-match in welding after anodic process.
The model ER5356 do not suggested to use in aluminium alloy workpiece which working temperature is over 65º C, thus will cause corrosion cracking in welded joints. You should strictly clean the oxide film on the edge of the workpiece and oil before welding, otherwise it will make bad weld produce and cause porosity, slag inclusion and other defects. And a plate can be used to hold molten metal to ensure meld form.
The argon arc welding of Aluminium & Magnesium alloy welding wires is used as the filler material, in welding among Al-Mg-Si, Almasilalloy and Aluminium & Magnesium alloy, like: Bicycles, aluminium scoter, etc. Engine carriage, pressure vessel, armory processing, ship-building. Space shuttle, etc.Widely Used Aluminum Alloy Wire Er4043, Er5356, Er5183, Er4047
Characteristic
Melting range 1060 - 1175°F
Electrical conductivity 29%IACS(O);27%IACS(H18)
Density 2.66g/mm3
Anti corrosion performance A(Gen) A(SCC)
The coefficient of thermal expansion (20 Degree ~300Degree) 23.7×10-6/K
Thermal conductivity (20 Degree)  110-150W/m@K

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now

You Might Also Like

Diamond Member Since 2018

Suppliers with verified business licenses

Manufacturer/Factory, Trading Company
Registered Capital
1000000 RMB
Plant Area
1001~2000 square meters