Customization: | Available |
---|---|
Type: | Rolling Wire |
Material: | Aluminum / Aluminum Alloy |
Still deciding? Get samples of US$ 20/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
AWS Code | Chemical Composition (%) | |||||||
Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | |
ER1060 | 0.25 | 0.35 | 0.05 | 0.03 | 0.03 | ~ | 0.06 | 0.03 |
ER1100 | 0.95 | 0.95 | 0.05-0.20 | 0.05 | ~ | ~ | 0.10 | ~ |
ER4043 | 4.5-6.0 | 0.80 | 0.30 | 0.05 | 0.05 | ~ | 0.10 | 0.20 |
ER4047 | 11.0-13.0 | 0.80 | 0.30 | 0.15 | 0.10 | ~ | 0.20 | ~ |
ER5356 | 0.25 | 0.40 | 0.10 | 0.05-0.20 | 4.5-5.5 | 0.05-0.20 | 0.10 | 0.06-0.20 |
ER5183 | 0.40 | 0.40 | 0.10 | 0.5-1.0 | 4.3-5.2 | 0.05-0.20 | 0.25 | 0.15 |
ER5556 | 0.10 | 0.30 | 0.05 | 0.55-8.0 | 4.7-5.2 | 0.05-0.10 | 0.09 | 0.05-0.10 |
Product Photos:
Product Description
Product Name | Custom Made Good Sales aluminium alloy welding wire er4043 er5356 |
Keywords | Aluminium alloy welding wire er4043 er5356 |
Material | Aluminium alloy |
Color | Silver |
Standard | AWSA 5-10 |
Grade | ER4043 ER5356 |
Size | Available Diameters:
0.8mm / 0.9mm/ 1.0mm / 1.2mm / 1.6mm / 2.0mm / 2.4mm etc.. |
Weight | 0.5kg/2kg/6kg /7kg per spool, or by bundle |
Used | Petrochemical engineering,fertilizer equipment |
Packing
Q1:Which filler wire is best for welding 6061 aluminum, 5356 or 4043?
A:Both are acceptable, but each has advantages and disadvantages depending on the application.
5356 aluminum alloy, which contains 5% Mg, is stronger and more ductile than 4043 generally.But 4043, containing 5% silicon, is more crack-resistant, easier to weld with, less prone to weld smut, and yields a more aesthetic weld.
Q2:If 5356 is stronger, shouldn't I always use it?
A:The answer is no.
4043 is less crack-sensitive than 5356 and shows less tendency for crater cracking.If your component will be heat-treated after welding, use 4043;5356 can be made susceptible to stress corrosion cracking after heat treatment.Similarly, if the component will operate at temperatures above 150 degrees F, use 4043 to avoid stress corrosion cracking.
But if the component will be anodized after welding, use 5356.The high silicon content of 4043 will cause the weld to turn black during anodizing, making the location of each weld obvious and unattractive;5356 will anodize to a silver color.
Wire Chemical Composition (%) | |||||||||||||
Category | Trademark | GB | AWS | Properties and Uses | |||||||||
Chemical Composition (%) | |||||||||||||
TIG | MIG | Cu | |||||||||||
Aluminum with | CJ-1100 | S301 | ER1100 | Plastic, corrosion resistant aluminum gas welding or TIG welding with. | |||||||||
0.05~0.20 | |||||||||||||
Corrosion resistantaluminum Alloy |
CJ-5183 | S331 | ER5183 | High strength, good corrosion resistance, aluminum welding use. | |||||||||
≤0.10 | |||||||||||||
CJ-5356 | S5356 | ER5356 | Good corrosion resistance, high strength, good versatility, aluminum welding use,especially for 5083 welding materials | ||||||||||
≤0.10 | |||||||||||||
CJ-4043 | S311 | ER4043 | Good corrosion resistance, versatility, large, aluminum welding, or weldingpurposes, not for high-magnesium alloy welding, welding materials used in the 4043better |